Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced N2U40G7 UN - PA9T FR - BASF

Material Data Center offers the following functions for Ultramid® Advanced N2U40G7 UN:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
The product is a halogen free flame retardant high temperature polyamide with high flowability, high temperature resistance for surface mount technology (SMT), excellent mechanical properties and high dimension stability, which all make it a perfect fit for E&E applications, especially various thin wall connectors and sockets.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 20 / * cm³/10min ISO 1133
Temperatura 325 / * °C -
Carico 2.16 / * kg -
Ritiro di stampaggio, parallelo 0.2 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.8 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 12500 / - MPa ISO 527
Carico unitario a rottura 150 / - MPa ISO 527
Deformazione a rottura 2 / - % ISO 527
Modulo a flessione, 23°C 12800 / - MPa ISO 178
Resistenza alla flessione 230 / - MPa ISO 178
Resistenza all'urto Charpy, +23°C 60 / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 13 / - kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 305 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 275 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 14 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 62 / * E-6/K ISO 11359-1/-2
Reazione al fuoco a spessore h V-0 / * class IEC 60695-11-10
Spessore provato 0.2 / * mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica >1E13 / - Ohm*m IEC 62631-3-1
Resistività superficiale * / >1E15 Ohm IEC 62631-3-2
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica 1490 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
Proprietà Specifiche Materialesecco/condUnitáNorma del test
ISO Data
Numero di viscosità 77 / * cm³/g ISO 307, 1157, 1628
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Forma fisica disponibile
Pellet, Colore naturale
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Stabilizzato o stabile al calore
Caratteristiche
Stabilità del colore
Applicazioni
IT / Apparecchiature per ufficio, Elettrotecnica ed electrici
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PROCESSING
injection molding, Melt temperature, range: 300 - 330 °C
injection molding, Mold temperature, range: 100 - 140 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.